1.2 EQUIPMENT PROCESS
a/ Spinning Process
Vacuum Dryer →Hopper →Screw Extruder→Filter→Spinning Beam→Metering Pump→Spinning→ Quenching Device→Finish Applicant→Winder→Drafter→Feeding Machine→Can Traversing Drive
b-1/ Post-spinning Process for hollow-crimped fiber
Creel Stand→Furl Stand→godet M/C→Immersion Oil Bath→First Drafter M/C→Water Bath →Second Drafter M/C→Steam Box→Third Drafter M/C→Stacker→Steam Box→Crimper M/C →Belt Conveyer→Oil Finishing Device→Tension Device→Cutter M/C→Spreader Device
→Relaxing Heat Setter→Chain Conveyer→Baler
b-2/ Post-spinning Process for cotton-type fiber
Creel Stand→Furl Stand→godet M/C→Immersion Oil Bath→First Drafter M/C→Water Bath →Second Drafter M/C→Steam Box→Third Drafter M/C→Stacker→Steam Box→Crimper M/C →Belt Conveyer→Spreader Device→Relaxing Heat Setter→Tension Device→Cutter M/C →Chain Conveyer→Baler
1.3 Specification:
Types of raw material: polyester chip virgin grade, chip off grade, and washed pet bottle flakes.
Type: single side, right or left hand.
Spec. of fiber: 1.5-20D.
Spinning speed: 600-1200m/min.
Space of the spinning position: 600mm, 750mm.
Spinning position: 4, 6, 8, 12, 16, 18, 24, 30.
Stretching speed: 50 ~ 280 m/min, Normal 240m/min.
Stretching Ratio: 2.5 ~ 4.5 times.
Driving type: united or single motor driving.
Fiber Length:32.8-301.6mm.